Most requests we get for plastic rod start the same way: which material should we use? The honest answer depends less on the grade itself than on where the finished part will actually sit.
Heat is usually the first filter
PEEK holds its stiffness at continuous service temperatures around 250 °C and tolerates short excursions higher. POM is comfortable to roughly 100–120 °C. Standard nylon softens earlier than either. A part mounted near a motor, or one that goes through steam sterilisation, often rules two of the three out immediately.
Moisture changes the tolerance
Nylon takes up water from humid air and wash cycles. The part grows slightly, which matters if you have machined a tight fit. POM absorbs far less and keeps its dimensions, which is why it turns up in gears and bushings. PEEK stays close to stable even in wet service.
Machining cost is part of material cost
POM cuts cleanly and finishes well, so it suits turned parts in quantity. Nylon is harder on tooling and prefers sharp cutters. PEEK is the slowest of the three to machine; rigid setups and moderate speeds help, but the extra time is real. Compare the finished-part cost, not just the price per kilo.
A practical shortlist
- Dry, steady, load-bearing parts at moderate cost: POM
- Impact resistance and wear in drier conditions: nylon
- High heat, aggressive chemicals or steam cleaning: PEEK
We keep rod in all three grades and cut to length. Share the working temperature, load and quantity, and our team will suggest a grade before you commit to a full order.